ASTM D3170/D3170M provides a standardized procedure for measuring the chipping resistance of coatings exposed to stones or other flying objects impacting a coated surface. This method employs a gravel-projecting machine, or gravelometer, to throw standardized road gravel against coated test specimens under controlled conditions. Lab testing can be conducted at room temperature or at a particularly low temperature to assess the coating behavior under service conditions. After gravel impact, clean up any dislodged or broken coating with tape, and count the resulting chips directly or compare them with chipping-rating references based on standard chip size. The method typically utilizes 102 × 305 mm (4 × 12 in.) test panels; however, the purchaser and the seller may agree on specimen composition, surface preparation, and size. ASTM D3170/D3170M (Standard Test Method for Chipping Resistance of Coatings) is like SAE J-400 and provides controlled impact conditions to improve reproducibility when laboratories compare coating systems.
Get Certified ASTM D3170/D3170M Testing for Reliable Coating Chipping Evaluation
ASTM D3170/D3170M testing helps laboratories assess coatings’ ability to resist damage from gravel, stones, and other flying objects. Automotive manufacturers and coating developers can use the results to compare coating systems and evaluate performance on surfaces exposed to road debris. The technique is especially helpful at low temperatures when flexibility of the coating may diminish, and chipping becomes more likely.
What is the scope of ASTM D3170/D3170M?
ASTM D3170/D3170M determines the resistance of coatings to chipping damage caused by stones or other flying objects. The technique sprays standardized road gravel onto coated samples under controlled air pressure and controlled temperature. Laboratories can then assess the damage numerically by the number of chips or by standard visual rating guides.
ASTM D3170/D3170M testing is used in laboratories to test the resistance of coatings to gravel and stone impact. Manufacturers use these results to compare coatings and understand whether a coating system can survive surface damage from impact.
This standard:
Evaluates automotive coating chipping resistance and supports comparison of different coating formulations.
Helps assess coatings used on surfaces exposed to road gravel and stones.
Supports coating-system development and optimization and helps evaluate the effect of low temperature on chipping resistance.
Coordinates quality control and acceptance testing and helps evaluate protective coating performance under controlled impact conditions.
Which Materials Can Be Tested Under ASTM D3170/D3170M?
ASTM D3170/D3170M applies to coatings applied to suitable test panels. The composition, preparation of the surface, and size of the specimen must be agreed upon between the seller and the purchaser. Usually, the standard employs coated panels that are 102 x 305 mm (4 x 12 in) in size.
Why is ASTM D3170/D3170M Important?
ASTM D3170/D3170M gives laboratories controlled impact conditions for comparing the chipping damage resistance of coatings. Chipping can damage the appearance of the coating and expose the substrate beneath. The process allows coating developers to assess coatings before field use.
ASTM D3170/D3170M Equipment and Sample Preparation Guide
This test specifies a gravel-projecting machine, standard gravel, temperature-conditioning equipment, adhesive tape, and test tools for evaluation of damaged coating. Laboratories should make representative coated panels and condition them at the desired test temperature before exposure.
Laboratories test coated panels with agreed composition, substrate preparation, coating system, and film condition. Test panels measuring 102 × 305 mm (4 × 12 in.) are commonly used.
Specimen Preparation
Technicians prepare the substrate and coating system according to the agreed coating specification. Control coating application, surface preparation, and aging conditions as required by the testing agreement.
Specimen Dimensions
The standard does not require one mandatory panel size. 102 × 305 mm (4 × 12 in.) panels are commonly used. The chip-evaluation area uses a centered 102 × 102 mm (4 × 4 in.) square.
Instrumentation
Gravelometer or gravel-projecting machine, graded road gravel, compressed-air supply, temperature-conditioning equipment or cold room/freezer, adhesive tape, appropriate measuring/evaluation equipment, transparent grid, chipping-rating standards, specimen holder, pressure controls, and timer.
ASTM D3170/D3170M Testing Procedure and Requirements
ASTM D3170/D3170M involves gravel impacting, removal, and testing of loose or damaged coating. Laboratories can use either cabinet-style or modular-style gravelometers. Other reference ASTM documents include D609, D823, D1005, D1186, D1400, D1733, and D2201. The complete procedure for ASTM D3170M is given as:
Technicians condition the coated specimens for at least 1 h at the specified test temperature. They maintain free access around the specimens to promote effective temperature equilibration.
Gravelometer Preparation
Analysts adjust the gravel apparatus air pressure to 480 ± 20 kPa (70 ± 3 psi) with the air valve open. They prepare 473 mL (1 US liquid pint) of graded gravel, approximately 250–300 stones.
Gravel Impact
Technicians place the conditioned coated specimen in the holder with the coated surface facing the front of the apparatus. They project the graded gravel against the specimen. For modular equipment, a typical test time is 10 s unless the contractual test requirement specifies otherwise.
Chip Removal and Evaluation
After impact, technicians allow specimens to return to room temperature, remove condensation, and use adhesive tape to remove loose or damaged coating. Analysts evaluate the central 102 × 102 mm (4 × 4 in.) area using chip counts or standardized chipping-rating references.
ASTM D3170/D3170M Testing Process and Data Collection
The technicians first make the coated test panels according to the agreed substrate, surface pre-treatment, coating application process, and aging conditions. They then condition the specimens for at least 1 h at the selected test temperature. They then operate the gravelometer with an air pressure of 480 ± 20 kPa (70 ± 3 psi) for the standard gravel procedure. Approximately 250-300 stones are added to 473 mL (1 US liquid pint) of graded road gravel. They place the conditioned panel in the specimen holder with the coated side against the gravel projection system. The apparatus then throws the gravel at the coating under controlled conditions. Technicians let the panel cool down after exposure and dry it. They place adhesive tape on the area to be evaluated and press it down. Then they take off the tape to peel off loose or damaged coating. Technicians repeat the tape-removal process in different directions until they remove the loose or damaged coating. Laboratories can evaluate the chipped area in two ways. The first method counts the number of chips in certain size ranges and is more precise. The second approach visually matches the damage to chipping rating standards.
ASTM D3170 Testing Procedure Using Gravelometer
ASTM D3170/D3170M Common Challenges and Troubleshooting
Chipping-resistance results may be different if the specimen conditioning, gravel characteristics, air pressure, exposure time, coating preparation, and evaluation procedures are not controlled. Common challenges include incorrect air pressure, incorrect gravel volume, improper gravel grading, poor temperature conditioning, incomplete gravel discharge, incorrect tape, inconsistent coating, incorrect evaluation, and subjective visual evaluation.
ASTM D3170/D3170M Analysis Results and Interpretation
The report summarizes the chipping resistance of the tested coating under the specified impact conditions. The results help engineers evaluate coating damage caused by stones or other flying objects and compare the observed chipping performance with applicable coating or product requirements.
Laboratories report results for temperature in °C, dimensions in mm, and air pressure of the gravelometer in kPa or psi.
The laboratory provides the chipping resistance rating or classification from the indicated test evaluation procedure along with the test conditions.
Analysts document the coating identification, test-panel information, impact-test configuration, test temperature when applicable, and observed chipping characteristics during evaluation.
Engineers compare the observed chipping resistance and damage characteristics with applicable coating or product requirements to evaluate the tested coating’s resistance to impact damage.
ASTM D3170/D3170M is a standard test method for determining the resistance of coatings to chipping damage from stones or other flying objects.
What equipment does ASTM D3170 use?
The method employs a gravel-projecting machine or gravelometer, graded road gravel, compressed air, a temperature-conditioning machine, adhesive tape, and chipping-evaluation tools.
What size test panel does ASTM D3170 use?
The standard states that specimen size should be agreed upon by the purchaser and seller. 102 × 305 mm (4 × 12 in.) panels are commonly used.
Laraib Hashmi is an aspiring research enthusiast and science content professional with a strong interdisciplinary skill set, holding a postgraduate degree in Applied Microbiology from KIIT Bhubaneshwar, Odisha. Know More
Testimonials
Real results
Engineers trust us with what matters most
“We had a great experience working with this company for our ASTM E84 testing. They were the first company to respond to our inquiry within just a few minutes of submitting it. From start to finish, the communication was excellent, and the entire process was swift, straightforward, and hassle-free.”
Ivars FancyWalls
United States
“Very good communication, testing associates were very patient with delays on our end. Reasonable turnaround time for results and nicely detailed report. Analysts were also quick to answer any follow-up questions. Happy with results.”
Skye Henderson
United States
“Matestlab connected us with an accredited lab within days, cutting weeks off our product validation timeline.”
Rebecca Kozodoy-Pins
United States
Why Choose Matestlab?
Matestlab is a unified testing services partner based in the USA. Matestlab offers raw material and product testing services through accredited, expert laboratories primarily based in the USA. Matestlab supports physical, thermal, chemical, electrical, mechanical, environmental, and characterization testing needs through its global network of 2200+ accredited testing laboratories. Matestlab's in-house materials science experts curate and design comprehensive testing programs matched to the sample material and specific testing need, with regulatory requirements and confidentiality in mind.
If you are looking for a managed and trusted testing partner to achieve your research goals, feel free to schedule a meeting with us or send us a request at connect@matestlabs.com to learn more about our services. For a quick quote, call us at (302)244-7710. We are happy to serve you.
Start Your Testing Project Today
Define your requirements and get access to specialized laboratories ready to deliver results